LaCrO3 powder has been synthesised at low temperature (700oC) by the combustion of gel prepared from polyvinyl alcohol (PVA) and metal nitrates. LaCrO3 characterization is examined by X-ray diffraction (XRD), thermogravimetric and differential thermal analysis (TG-DTA), field emission scanning electron microscopy (FESEM)and BET (Brunaure-Emmet-Teller) measurements. The obtained sample under optional preparative conditions has nano scale with relatively large specific square area ( ~14 m2/g).
Đại và cộng sự, L. M. (2014). Tổng hợp perovskit LaCrO3 bằng phương pháp đốt cháy gel ở nhiệt độ thấp. Vietnam Journal of Chemistry, 46(1), 83–88. https://doi.org/10.15625/4276